1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-2J57

Alternate Names: 2J57,2J-57

Description: High expansion low melting phosphate based glass

Oxide Analysis Formula Tolerance
Li2O 3.60% 0.26
Na2O 21.30% 0.74
B2O3 6.60% 0.20
Al2O3 19.20% 0.41
41.00% -
SiO2 1.20% 0.04
F 7.20% 0.82
Oxide Weight 127.27
Formula Weight 127.27

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 21.00
Co-efficient of Linear Expansion 21.00 (50-450C)
Frit Softening Point 980F
Frit Melting Range (C) 950-1000F
I.F.P. (celsius) 355C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy