Pemco Frit P-1X24

Alternate Names: 1X-24,1X24

Notes

Developed for partially-fritted texture glaze to be used with Pb-1X22.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Pemco Frit Pb-1X22
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.