Pemco Frit P-1A43

Alternate Names: 1A43,1A-43

Description: Low expansion high zinc borosilicate

Oxide Analysis Formula Tolerance
ZnO 65.30% 1.00
B2O3 18.60% 0.33
SiO2 16.10% 0.33
Oxide Weight 124.66
Formula Weight 124.66

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1A44
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 3.50
Co-efficient of Linear Expansion 3.50 (50-450C)
Frit Softening Point 2000F
Frit Melting Range (C) 1950-2070F
I.F.P. (celsius) 660C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy