Physical Properties: ------------------------------------
Ultimate Crystal Size, microns: 3-4 3-4 3-4
BET surface area, sq m per g: 0.6 0.6 0.4 13
Blaine surface area, sq cm/g: 5200 5200 4400
LOI, 20C-1000C: 0.13 0.12 0.12 0.5