Alternate Names: NiO, Nickelous oxide, Green Nickel Oxide, Nickel(II) oxide
Formula: NiO
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| NiO | 100.00% | 1.00 | |
| Oxide Weight | 74.70 | ||
| Formula Weight | 74.70 | ||
| Oxides | NiO - Nickel Oxide |
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Typecodes |
Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials. |
| URLs |
http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc09/icsc0926.htm
Nickel Oxide Hazards at ilo.org |
| URLs |
https://en.wikipedia.org/wiki/Nickel(II)_oxide
Green Nickel Oxide at Wikipedia |
| Hazards |
Nickel Compounds Toxicity
|
| Materials |
Nickel Oxide Black
|
| Materials |
Nickel Carbonate
|
| Frit Softening Point | 1984C |
|---|---|
| Density (Specific Gravity) | 6.6- 7.5 |