Na and Li Metaborate Eutectic

Oxide Analysis Formula Tolerance
Li2O 10.40% 0.41
Na2O 30.70% 0.59
B2O3 58.90% 1.00
Oxide Weight 118.46
Formula Weight 118.46

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 640