Na & Sr Metasilicate Eutectic

Formula: SrSiO3 . 5.33Na2SiO3

Oxide Analysis Formula Tolerance
Na2O 40.50% 0.84
SrO 12.60% 0.16
SiO2 46.90% 1.01
Oxide Weight 129.06
Formula Weight 129.06

Related Information

Links

Glossary Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures.
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.