1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Mulcoa 47 Calcine Grog

Description: Mullite grog

Oxide Analysis Formula Tolerance
Al2O3 46.80% 1.00
SiO2 50.00% 1.81
TiO2 1.90% 0.05
Fe2O3 0.95% 0.01
Oxide Weight 217.19
Formula Weight 217.19

Notes

A number of grades are available and are used in the refractory industry.

Related Information

Links

Materials Grog
Materials Mulcoa 60 Calcine Grog
Materials Mulcoa 70 Mullite
Typecodes Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy