Description: Fritte au zinc

Oxide Analysis Formula Tolerance
MgO 2.99% 0.12
ZnO 38.77% 0.77
Na2O 4.22% 0.11
Al2O3 5.68% 0.09
SiO2 40.15% 1.08
B2O3 8.18% 0.19
Oxide Weight 161.65
Formula Weight 161.65

Notes

Corrected this chemistry Oct 2022, it was:
Na2O 4.0, ZnO 39.0, MgO .12, Al2O3 .095, SiO2 1.077

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 590C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy