Moulin Fritte M759

Description: Fritte boro-alcaline

Oxide Analysis Formula Tolerance
Na2O 16.07% 1.00
B2O3 36.43% 2.02
SiO2 47.50% 3.05
Oxide Weight 385.81
Formula Weight 385.81

Notes

Corrected chemistry Oct 2022, it was:
Na2O 15.0, Al2O3 51.0, SiO2 34.0

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 548C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy