Description: Fritte plombo-boracique

Oxide Analysis Formula Tolerance
PbO 62.30% 1.00
B2O3 29.30% 1.51
SiO2 8.40% 0.50
Oxide Weight 358.27
Formula Weight 358.27

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 495C