Magnesia-Alumina-Silicate Eutectic

Oxide Analysis Formula Tolerance
MgO 20.00% 1.00
Al2O3 20.00% 0.40
SiO2 60.00% 2.01
Oxide Weight 201.50
Formula Weight 201.50

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1350C