1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Li Metaborate and Li Metasilicate Eutectic

Oxide Analysis Formula Tolerance
Li2O 30.90% 1.00
SiO2 18.70% 0.30
B2O3 50.40% 0.70
Oxide Weight 96.44
Formula Weight 96.44

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 802C