| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 77.80% | 1.00 | |
| B2O3 | 5.80% | 0.24 | |
| SiO2 | 16.40% | 0.78 | |
| Oxide Weight | 286.89 | ||
| Formula Weight | 286.89 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 485C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |