Laterite Red Clay

Alternate Names: IMCO Laterite

Oxide Analysis Formula Tolerance
SiO2 43.00% 2.28
Al2O3 32.00% 1.00
Fe2O3 23.00% 0.46
TiO2 2.00% 0.08
LOI 11.00%n/a
Oxide Weight 318.75
Formula Weight 358.15

Notes

Laterites are products of intense and prolonged chemical weathering, most commonly associated with tropical and subtropical environments. During the process, soluble and mobile components such as Na, K, Ca and Mg are strongly depleted and silica can also be progressively removed. Iron and aluminum become residually concentrated. Thus laterites are not defined by a specific chemistry or mineralogy; their composition depends on the parent rock, climate, drainage and degree of weathering.

Typical laterite mineral assemblages contain varying proportions of kaolinite, goethite, hematite, gibbsite and residual quartz. Some can contain extraordinary amounts of iron, while strongly aluminous ones grade toward bauxitic materials. This mineralogical variation means that chemical analyses alone do not reveal how the Al2O3 and Fe2O3 are actually hosted.

Laterites are often refractory because the weathering process that forms them removes many of the alkali and alkaline-earth oxides that normally act as ceramic fluxes. Thus an iron-rich laterite can be much more refractory than an ordinary red-burning sedimentary clay having a similar Fe2O3 content. This material, for example, has a reported pyrometric cone equivalent of 19 despite its very high iron content.

Plasticity is variable. Strongly laterized, oxide-rich or concretionary materials can have little plasticity, whereas kaolinite-rich lateritic clays can be plastic. In ceramics these materials can be useful as unusual sources of iron and alumina in red- and dark-burning bodies and as additions where their combination of high iron content and refractoriness is desirable.

The published analysis for this example IMCO material requires interpretation: the listed SiO2, Al2O3, Fe2O3 and TiO2 already total 100%, before the reported 11% LOI is added. The oxide values may therefore have been reported on a calcined basis rather than as a conventional analysis including LOI.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://www.clayimco.com/industrial-clays
IMCO information on their mined clays

Data

Pyrometric Cone Equivalent 19

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy