1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Keramikos Fritte M1

Description: Borax Fritte

Oxide Analysis Formula Tolerance
CaO 7.00% 0.35
SiO2 56.00% 2.58
MgO 3.00% 0.21
Al2O3 11.00% 0.30
B2O3 12.50% 0.50
Na2O 10.00% 0.45
Oxide Weight 276.00
Formula Weight 276.00

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Frit Melting Range (C) 850-1060C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy