| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 50.71% | 1.00 | |
| SiO2 | 45.92% | 1.54 | |
| LOI | 3.38% | n/a | |
| Oxide Weight | 194.37 | ||
| Formula Weight | 201.16 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |