1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Hommel Frit 573

Description: High lead zinc frit

Oxide Analysis Formula Tolerance
Na2O 1.20% 0.04
ZnO 19.75% 0.47
PbO 57.05% 0.49
Al2O3 1.96% 0.04
SiO2 20.03% 0.64
Oxide Weight 193.19
Formula Weight 193.19

Related Information

Links

Materials Pemco Frit Pb-740
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.6 x 10-6
Frit Softening Point 1560F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy