Hommel Frit 550

Description: Leadless calcium borax frit

Oxide Analysis Formula Tolerance
CaO 16.99% 0.68
Na2O 8.80% 0.32
B2O3 18.69% 0.60
Al2O3 4.99% 0.11
SiO2 50.52% 1.89
Oxide Weight 224.80
Formula Weight 224.80

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-103
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.50
Co-efficient of Linear Expansion 8.5 x 10-6
Frit Softening Point 1650F
Frit Melting Range (C) 1650F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy