Glasurfritten 35.2

Alternate Names: 35 2,35-2

Description: Bleihaltige Zinkmatt-Fritte

Oxide Analysis Formula Tolerance
PbO 23.00% 0.19
CaO 5.00% 0.16
Na2O 2.00% 0.06
ZnO 27.00% 0.60
B2O3 4.00% 0.10
Al2O3 2.00% 0.04
SiO2 37.00% 1.11
Oxide Weight 179.82
Formula Weight 179.82

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 61 x 10-7
Frit Softening Point 600C
Frit Melting Range (C) 970-1030C
By Tony Hansen