Alternate Names: Silicon dioxide, silica, quartz sand

Formula: SiO2

Oxide Analysis Formula Tolerance
SiO2 100.00% 678.87
Al2O3 0.25% 1.00
Oxide Weight 40,902.00
Formula Weight 40,902.00

Notes

Used in glass containers, flat glass, fiber glass insulation, frit production and a variety of other specialty glass products. We have included a token impurity just as a reminder that these products are not completely pure.

Related Information

Links

Materials Edgar Glass Sand
Materials Crystalline Silica
Materials Silica
Silica, sold as a white powder, is pure quartz mineral. Quartz is pure SiO2 silicon dioxide. It is the most abundant mineral on earth and most used in ceramics.
URLs http://www.u-s-silica.com/msds.htm
Example of a glass sand MSDS
URLs https://www.ussilica.com/
U.S. SILICA Website
URLs https://www.ilo.org/global/topics/safety-and-health-at-work/resources-library/publications/WCMS_118100/lang--en/index.htm
Crystalline silica in respirable airborne dusts at International Labour Organization
URLs http://en.wikipedia.org/wiki/Quartz
Quartz on WikiPedia
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
Oxides SiO2 - Silicon Dioxide, Silica

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy