1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

General Frit GF-111

Alternate Names: Frit 111, Frit GF111

Description: SODIUM CALCIUM BOROSILICATE

Oxide Analysis Formula Tolerance
CaO 20.04% 0.68
Na2O 10.28% 0.32
B2O3 23.30% 0.64
SiO2 46.37% 1.48
Oxide Weight 191.18
Formula Weight 191.18

Notes

A lime and borate source in partially fritted glazes, lead bisilicate glazes and low cost hobby glazes cone 02-10.

Low alumina makes room for blending kaolin to harden the glaze and impart excellent application properties.

See also: TAM C-14

Related Information

Links

Materials Hommel Frit 242
Materials Pemco Frit P-54
Materials Fusion Frit F-12
Materials Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.60
Frit Softening Point 1450F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy