Fusion Frit F-77

Alternate Names: Frit F77

Description: BOND FRIT

Oxide Analysis Formula Tolerance
CaO 18.00% 0.61
MgO 4.30% 0.20
Na2O 6.20% 0.19
B2O3 45.00% 1.23
Al2O3 2.50% 0.05
SiO2 24.00% 0.76
Oxide Weight 189.55
Formula Weight 189.55

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-309
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy