Fusion Frit F-577

Alternate Names: Fusion Frit F577

Description: Calcium magnesium zirconium matt frit

Oxide Analysis Formula Tolerance
Na2O 1.50% 0.04
CaO 15.50% 0.45
MgO 12.60% 0.51
Al2O3 3.50% 0.06
B2O3 6.40% 0.15
SiO2 55.00% 1.49
ZrO2 5.50% 0.07
Oxide Weight 163.09
Formula Weight 163.09

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.8 x 10-6
Frit Softening Point 1700F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy