1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-498

Alternate Names: Fusion Frit F498

Description: High magnesium flux

Oxide Analysis Formula Tolerance
MgO 10.00% 0.43
Na2O 3.60% 0.10
CaO 15.50% 0.47
Al2O3 10.50% 0.18
B2O3 16.60% 0.41
SiO2 43.80% 1.25
Oxide Weight 171.68
Formula Weight 171.68

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.92 x 10-6
Frit Softening Point 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy