Frit Fsb656

Description: Lead Bisilicate Frit

Oxide Analysis Formula Tolerance
PbO 65.00% 1.00
SiO2 35.00% 2.00
Oxide Weight 343.38
Formula Weight 343.38

Notes

One of the few frits available to potters in South Africa. Sold at http://www.potters.co.za. We have set the standard lead bi-silicate chemistry (the chemistry is not published at their website).

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1080C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy