1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit Fsb571

Description: Leadless Calcium Borosilicate Frit

Oxide Analysis Formula Tolerance
SiO2 56.50% 4.10
Al2O3 12.00% 0.51
B2O3 18.00% 1.13
Na2O 3.50% 0.25
MgO 0.50% 0.05
CaO 9.00% 0.70
Oxide Weight 433.96
Formula Weight 433.96

Notes

One of the few frits available to potters in South Africa. It is similar to 3124 and 3195 but with less KNaO and CaO (likely a higher temperature).

Chemistry not given on suppliers website, this was found at https://glazy.org/materials/15513

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy