Frit A 1316

Description: Reimbold & Strick lead monosilicate frit

Oxide Analysis Formula Tolerance
SiO2 21.20% 1.00
PbO 78.80% 1.00
Oxide Weight 283.25
Formula Weight 283.25

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Ferro Frit 3377
Materials Lead Monosilicate Frit
A standard frit of 1 molar part of PbO and 1 of SiO2. It melts lower than a lead bisilicate.
URLs http://www.reimbold-und-strick.de/en/index-eng/
Reimbold & Strick website

Data

Co-efficient of Linear Expansion 90 x 10-7 (20-400C)
Frit Softening Point 470C
Glass Transition Temperature 440C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy