Frit 439

Alternate Names: MexGBSub F439

Description: Gerstley Borate Substitute

Oxide Analysis Formula Tolerance
SiO2 13.89% 0.29
B2O3 41.32% 0.75
Al2O3 1.62% 0.02
Na2O 7.97% 0.16
MgO 4.95% 0.16
CaO 30.26% 0.68
Oxide Weight 126.47
Formula Weight 126.47