Flint Pebbles

Notes

These are a light grey in appearance and are manufactured from large monolithic boulders which are broken down, ball milled to smooth and round each pebble and then hand picked to eliminate culls.

They have a density of 2.6 and a Moh hardness of 7.5. They are used in ball mills.