Alternate Names: Fe (II) Oxalate Dihydrate
Description: FeC2O4 - 2H2O
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| FeO | 36.70% | 1.00 | |
| LOI | 63.29% | n/a | |
| Oxide Weight | 81.80 | ||
| Formula Weight | 222.83 | ||
CAS #: 6047-25-2
Formula weight: 179.90 (Anhydrous FW: 143.87)
Somewhat hygroscopic -- keep in sealed container.
This material is being researched by Jon Singer as a secret to the production of a copper red glaze. His comments are:
-Oxalic acid sublimes at 157C.
-This is Ferrous, so if you knock off the waters and the oxalic acid you get FeO, FW 71.844.
The LOI should be 60.06%.
-There is reason to believe that this material causes some _in-situ_ reduction.
-If I make a Copper Red glaze with this stuff, it reds up beautifully; if I make essentially the same
glaze with FeO, it mostly just turns pink. OTOH, that could be caused by some other kind
of magic going on.)
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Decomposition Temperature | 190C (Alfa) or 150C (CRC Handbook) |
|---|---|
| Density (Specific Gravity) | 2.28 |