Ferro Richoux Frit 21 C003

Alternate Names: Frit 21 C003

Description: Fritte Boracique

Oxide Analysis Formula Tolerance
Na2O 5.43% 0.40
CaO 3.69% 0.30
MgO 2.21% 0.25
ZnO 0.89% 0.05
Al2O3 6.70% 0.30
B2O3 15.25% 1.00
SiO2 65.83% 5.00
Oxide Weight 456.35
Formula Weight 456.35

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1030-1180C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy