Ferro Frit 90710F

Alternate Names: Bismuth frit

Notes

SiO2: 30% – 60%
B2O3: 6% - 10%
Al2O3: 8% - 15%
Na2O: 3% - 8%
CaO: 3% - 10%
Bi2O3: 15% - 30%

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.