Ferro Frit 90 740 F

Alternate Names: Frit 90740F

Description: Glass bonding frit, glass frit

Notes

Lead, cadmium, zinc and barium free glass: Li2O (5-20%), F (<5%), B2O3 (>20%), SiO2 (>20%), ZrO2 (>20%), TiO2 (<5%).
Suitable for sintered glass and for special applications, especially for abrasive grinding wheel applications.
Good acid and base resistance.
Softens at 680C (1256F).
CTE: 77

Related Information

Links

Oxide Analysis Formula Tolerance
URLs https://digitalfire.com/4sight/datasheets/TDS_90740F_EN_03_2017.pdf
Ferro Frit 90 740 F Glass Frit data sheet
URLs https://www.ferro.com/-/media/files/resources/industrial-specialty-materials/technical/ferro-industrial-specialty-materials-specialty-glass-frits-for-super-abrasive-grinding-wheels.pdf
Ferro Glass Bonding Frits
Materials Ferro Frit 90 741 F
Materials Ferro Frit 90 742 F
Typecodes Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy