1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 4171

Alternate Names: Frit 1057, Frit 3271, Frit DA4171

Description: Leadless calcium borosilicate frit (was Frit 3271, Frit 1057)

Oxide Analysis Formula Tolerance
CaO 11.00% 0.49
Na2O 12.80% 0.51
B2O3 21.60% 0.77
SiO2 54.60% 2.26
Oxide Weight 248.43
Formula Weight 248.43

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 49
Materials Glostex Frit H-2
Materials Ferro Frit 1057
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.30
Frit Softening Point 558C
Frit Melting Range (C) 1040-1100C
Glass Transition Temperature 590C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy