1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3851

Description: High magnesia leadless boron-free low expansion frit

Oxide Analysis Formula Tolerance
CaO 0.50% 0.01
MgO 23.80% 0.99
Al2O3 26.80% 0.44
SiO2 48.90% 1.36
Oxide Weight 166.81
Formula Weight 166.81

Notes

Used as a filler in resin bonded abrasives, an MgO source. Very high fire frit with very low expansion at cone 10.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.20
Frit Melting Range (C) 2400F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy