Ferro Frit 3304

Alternate Names: F3304

Description: High lead zincless frit for clear glaze cone 04-08

Oxide Analysis Formula Tolerance
Na2O 1.10% 0.07
PbO 54.40% 0.93
Al2O3 4.00% 0.15
SiO2 40.50% 2.58
Oxide Weight 382.45
Formula Weight 382.45

Notes

Made from flint, soda, clay and lead.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 61
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.6 x 10-6
Frit Melting Range (C) 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy