Ferro Frit 3225

Description: Low expansion cone 04 frit for vitrified bonded abrasives

Oxide Analysis Formula Tolerance
CaO 0.30% 0.07
MgO 0.20% 0.06
Na2O 4.40% 0.87
B2O3 21.90% 3.87
Al2O3 8.20% 0.99
SiO2 65.00% 13.31
Oxide Weight 1,230.34
Formula Weight 1,230.34

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 3GF272B
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.00
Frit Melting Range (C) 1650

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy