Ferro Frit 1081

Description: Insoluble colemanite substitute

Oxide Analysis Formula Tolerance
CaO 27.05% 1.00
B2O3 50.35% 1.50
Al2O3 4.92% 0.10
SiO2 17.68% 0.61
Oxide Weight 207.39
Formula Weight 207.39

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Materials Ferro Frit 2244
Materials Ferro Frit 2954
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1050-1160C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy