Erbium Oxide

Alternate Names: Lanthanide

Oxide Analysis Formula Tolerance
Er2O3 100.00% 1.00
Oxide Weight 382.50
Formula Weight 382.50

Notes

This is a lanthanide rare earth oxide, it is available as a raw powder.
It is used in ceramics as a colorant and can have an opacifying effect.

For information on making vibrant colors using lanthanides visit the page by David Pier linked to this record.

Quote from David Pier: "The oxide is a light baby pink color. It is the most expensive, the densest, and the weakest of these three colorants, but the only way you will ever get a transparent pink. Erbium oxide's density means it is absolutely essential that you use CMC gum. Erbium oxide gives its best pink color at concentrations of 8-10%, but it is difficult to get more than 8% to fully dissolve in the melt. It has given a more lavender color in the presence of iron traces in reduction."

Related Information

Links

URLs http://www.lagunaclay.com/news/rare.htm
New glaze colors using lanthanides
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy