DK-1 Monoclinic Zirconium Powder

Description: DK-2, DK-3, RC100

Oxide Analysis Formula Tolerance
Al2O3 0.03% 1.00
Fe2O3 0.04% 0.85
SiO2 0.04% 2.26
ZrO2 99.50%
TiO2 0.10% 4.26
Oxide Weight 339,014.00
Formula Weight 339,014.00

Notes

Particle size ranges from 0.90 microns to 8.0 microns, surface area from 3 to 100 grams to square meter.

Stabilized, partially stabilized and doped zirconias also available.

Related Information

Links

Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy