Description: Anti bacterial, mold and virus agent

Notes

A liquid available at drug stores. It contains 5% chloroxylenol (C8H9ClO), an aromatic and poisonous chemical (the remainder is pine oil, isopropanol, castor oil, soap and water). It is a potent antimicrobial against bacteria, mold and virus and should be added to glazes during the mixing process. We do not have a recommended amount, but it has a powerful odor, one that you will recognize from the hospital (they use it for cleaning). If your glaze smells like a hospital, then you likely put too much in!

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Biocide
These are added to glazes and bodies to prevent the growth of micro organisms. Often targeted at bacteria, mold or fungi.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy