Desulco Graphite

Description: Carbon

Formula: C

Notes

This product is 99.9% carbon with minuscule ash, gas, and sulfur content. It is especially useful in the production of high strength metals and other products where exceptional carbon purity is needed. This material can be recognized by its porosity, lower particle density and matte luster.

Graphite is made by firing various carbon sources to very high temperatures (up to 2500C). However Desulco products are made from processing petroleum products, producing a more consistent result.

It remains stable under extremely high temperatures without melting.

Quality graphite products are refined to remove gases and other impurities.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Graphite
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy