Denver Fireclay

Oxide Analysis Formula Tolerance
CaO 6.20% 1.00
Al2O3 11.50% 1.02
SiO2 59.80% 9.00
Fe2O3 4.10% 0.23
LOI 10.40%n/a
Oxide Weight 738.35
Formula Weight 824.05

Related Information

Links

Materials Fireclay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

Data

Frit Softening Point 2950F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy