Degussa Frit 90378

Oxide Analysis Formula Tolerance
ZnO 1.09% 0.05
Na2O 6.64% 0.40
CaO 8.26% 0.55
Al2O3 8.19% 0.30
SiO2 62.77% 3.90
B2O3 13.05% 0.70
Oxide Weight 373.52
Formula Weight 373.52

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 570C
Heating Microscope Analysis for Frits 785C
Heating Microscope Analysis for Frits 980C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy