Degussa Frit 90368

Alternate Names: Frit D-90368, Erdalkaliborsilikat D 90368

Oxide Analysis Formula Tolerance
MgO 1.87% 0.10
CaO 18.24% 0.70
Na2O 5.76% 0.20
Al2O3 11.84% 0.25
SiO2 55.82% 2.00
B2O3 6.46% 0.20
Oxide Weight 215.29
Formula Weight 215.29

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 76 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 630C
Heating Microscope Analysis for Frits 830C
Heating Microscope Analysis for Frits 1080C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy