Degussa Frit 90352

Oxide Analysis Formula Tolerance
Na2O 3.92% 0.10
CaO 7.09% 0.20
ZnO 28.27% 0.55
PbO 21.14% 0.15
SiO2 34.16% 0.90
B2O3 2.20% 0.05
Al2O3 3.22% 0.05
Oxide Weight 158.32
Formula Weight 158.32

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 483C
Heating Microscope Analysis for Frits 730C
Heating Microscope Analysis for Frits 970C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy