Degussa Frit 90328

Oxide Analysis Formula Tolerance
MgO 0.35% 0.10
CaO 0.24% 0.05
Na2O 4.52% 0.85
Al2O3 7.88% 0.90
SiO2 65.51% 12.69
B2O3 21.50% 3.60
Oxide Weight 1,164.60
Formula Weight 1,164.60

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 48 X 10-7 (20-400C)
Heating Microscope Analysis for Frits 495C
Heating Microscope Analysis for Frits 795C
Heating Microscope Analysis for Frits 1270C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy