Degussa Frit 90242

Alternate Names: Bleisilikat

Oxide Analysis Formula Tolerance
Al2O3 7.15% 0.25
PbO 62.54% 1.00
SiO2 30.31% 1.80
Oxide Weight 356.89
Formula Weight 356.89

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 82 x 10-8 (20-400C)
Heating Microscope Analysis for Frits 540C
Heating Microscope Analysis for Frits 750C
Heating Microscope Analysis for Frits 900C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy