Degussa Frit 90226

Alternate Names: Alkalibleiborfritte

Description: Alkaiblei-bortritte

Oxide Analysis Formula Tolerance
Al2O3 7.15% 0.25
PbO 62.54% 1.00
SiO2 30.31% 1.80
Oxide Weight 356.89
Formula Weight 356.89

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 117 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 473C
Heating Microscope Analysis for Frits 650C
Heating Microscope Analysis for Frits 800C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy